440C asye pur se yon gwo-kabòn martensitic asye pur li te ye pou dite ekselan li yo, rezistans mete, ak modere rezistans korozyon . Li se souvan itilize nan aplikasyon ki mande gwo fòs ak rezistans, tankou kouver, BEARINGS, mwazi, ak enstriman chirijikal {{3}
Voye rechèch
Dekri teren

440C Fèy asye pur - Pwopriyete Kle:

Klas:AISI 440C / UNS S44004

Konpozisyon:

Kabòn (C): 0.95-1.20%

CHROMIUM (CR): 16–18%

Manganèz (MN): mwens pase oswa egal a 1.00%

Silisyòm (Si): mwens pase oswa egal a 1.00%

MOLYBDENUM (MO): Mwens pase oswa egal a 0.75% (si ou vle)

Fosfò (P) & souf (s): mwens pase oswa egal a 0.04%

Dite:

Rkwit: ~ Hb 269

Fè tèt di toujou & apeze:HRC 56-60(Ka rive jwenn jiska HRC 62 ak tretman chalè apwopriye)

Rezistans korozyon:Bon (men enferyè a 304/316 asye pur akòz kontni kabòn segondè)

Mayetik:Wi (estrikti martensitik)

Aplikasyon komen nan 440C fèy pur:

✔ Lam kouto & kouver
Belings boul & pati valv yo
✔ Konpozan endistriyèl wo-mete
✔ Enstriman chirijikal ak dantè
✔ Mwazi foure & outillage

Fòm ki disponib & gwosè (tipik):

Epesè:0.1mm - 6mm (0.004 " - 0.25") oswa koutim

Lajè:Jiska 1500mm (59 ")

Fini sifas:Frèt-woule, rkwit, poli (e . g ., #4 fwote, glas)

Rekòmandasyon tretman chalè:

Rkwir:Chofe nan815-870 degre (1500-1600 degre f), dousman fre (~ 15 degre /h)

Redi:Chofe nan1010-1065 degre (1850-1950 degre f), lwil oliv oswa lè pasè

Tanperaman: 150-370 degre (300-700 degre F)pou pi bon dite

Machining & Fabrication Nòt:

Machinabilite:San Patipri (menm jan ak lòt asye pur difisil) - Sèvi ak zouti carbure

Weldability:Pòv (Chofe & Post-Weld Tretman Chalè Rekòmande)

 